Grinding process applied to workpieces with different
2020 2 25 After the workpiece grinding process an AISI 1020 steel cylinder 30 mm diameter and 100 mm length with 90 ± 2 HRB / 192 ± 40 HV soft steel was ground with a cut depth of 1 mm 10 cycles of 0.1 mm feed rate of 0.25 mm/min and spark out time of 5 s. Thus the wear profile of the grinding wheel was printed on the surface of AISI 1020